Method for fabricating optical fiber preform and method for fabricating optical fiber using the same
Abstract
Disclosed are a method for fabricating an optical fiber preform and a method for fabricating an optical fiber using the optical fiber preform. The method for fabricating the optical fiber preform including the steps of: (a) growing a first soot preform on a starting member by a soot deposition; (b) dehydrating the first soot preform; (c) sintering the first dehydrated soot preform to obtain a first glassed optical fiber perform; (e) growing an over-clad soot layer on the first optical fiber preform by soot deposition to obtain a second soot preform; and (f) sintering the second soot preform so as to obtain a second optical fiber preform which is glassed, wherein an average density of the first soot preform is substantially within a range of 0.190.30 g/cc, and the average density of the over-clad soot layer is substantially within a range of 0.50.75 g/cc.
Filed on: 2006-10-19; Application Number: 11583270
Applicant(s)
Mun Hyun DoJin Seong Yang
Jin Han Kim
Myung Hwan Pyo